不管在建筑行業(yè)、造船行業(yè)、家具行業(yè)、電氣行業(yè)中都離不開彩鋼板,但同時(shí)彩鋼板的發(fā)展也正在不斷地進(jìn)行創(chuàng)新,雖彩鋼板的性能很好,但在特殊情況下偶爾也會(huì)出現(xiàn)部分問題。而彩鋼板“爆漆”現(xiàn)象就是比較常見的,今天濟(jì)南彩鋼板房的小編給大家解析彩鋼板爆漆的原因
No matter in the construction industry, shipbuilding industry, furniture industry, electrical industry are inseparable from color steel plate, but at the same time, the development of color steel plate is also constantly innovative. Although the performance of color steel plate is very good, some problems will occasionally appear in special cases. And color steel plate "paint" phenomenon is more common, today's Jinan color steel panel room for everyone to analyze the causes of color steel plate paint explosion
1、配槽過程中,要加鈍化液后加水,因?yàn)殁g化液密度問題,會(huì)導(dǎo)致原料混合不均勻,從而會(huì)出現(xiàn)鈍化層與基板附著力差,讓彩鋼板表面出現(xiàn)爆漆現(xiàn)象。
1. In the process of tank preparation, water should be added after adding passivation solution. Due to the density of passivation solution, raw materials will be mixed unevenly, resulting in poor adhesion between the passivation layer and the substrate, resulting in paint explosion on the surface of color steel plate.
2、化板溫生茶工藝規(guī)定為2h一次,主要因?yàn)橄嚓P(guān)作業(yè)人員沒有定時(shí)對(duì)鈍化板溫度進(jìn)行跟蹤。特別在冬季,2h內(nèi)的溫度變化很大,從而會(huì)導(dǎo)致彩鋼板失效,在壓型時(shí)會(huì)出現(xiàn)因劃傷而掉漆的現(xiàn)象。
2. The chemical plate temperature raw tea process is required to be once every 2 hours, mainly because the relevant operators did not regularly track the temperature of the passivation plate. Especially in winter, the temperature changes greatly within 2 hours, which will lead to the failure of color steel plate and the phenomenon of paint dropping due to scratch during molding.
3、生產(chǎn)彩鋼板過程中,出口檢查鏡上有灰塵,部分棍子同樣有灰塵的存在。而灰塵會(huì)直接影響彩鋼板表面質(zhì)量,起初不會(huì)表現(xiàn)出來,但經(jīng)過長(zhǎng)時(shí)間的使用或經(jīng)過陽光的暴曬后,就會(huì)出現(xiàn)爆漆現(xiàn)象。
3. During the production of color steel plate, there is dust on the exit inspection mirror, and some sticks also have dust. Dust will directly affect the surface quality of color steel plate, which will not show at first, but after a long time of use or after exposure to the sun, the phenomenon of paint explosion will appear.
以上便是彩鋼板出現(xiàn)爆漆的三種情況,我們?cè)谄綍r(shí)一定要注意這些問題,正確合理的存放和使用彩鋼板,從而避免爆漆現(xiàn)象。想要了解更多內(nèi)容歡迎咨詢
濟(jì)南彩鋼板房http://nhmmgs.com官網(wǎng)。
The above are the three cases of paint explosion on color steel plate. We must pay attention to these problems at ordinary times, store and use color steel plate correctly and reasonably, so as to avoid paint explosion. For more information, welcome to consult Jinan color steel panel roomhttp://nhmmgs.com Official website.